MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 2091-T8x
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: These values for 0% cold work.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2091-T8x; AlLi; Aluminum Lithium Alloy; AA2091-T8x; UNS A92091; Al2091-T8x
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.58 g/cc0.0932 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 115115500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 146146Converted from Brinell Hardness Value
Hardness, Rockwell A 45.645.6Converted from Brinell Hardness Value
Hardness, Rockwell B 7171Converted from Brinell Hardness Value
Hardness, Vickers 130130Converted from Brinell Hardness Value
Tensile Strength, Ultimate 430 MPa62400 psi
Tensile Strength, Yield 330 MPa47900 psi
Elongation at Break 18 %18 %
Modulus of Elasticity 75.0 GPa10900 ksi
Fatigue Strength 80.0 MPa
@# of Cycles 1.00e+8
11600 psi
@# of Cycles 1.00e+8
Notched with Kt = 1.035
Shear Strength 260 MPa37700 psiCalculated value.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.9 µm/m-°C
@Temperature 20.0 - 100 °C
13.3 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.860 J/g-°C
@Temperature 100 °C
0.206 BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity 84.0 W/m-K583 BTU-in/hr-ft²-°F
Melting Point 560 - 670 °C1040 - 1240 °F
Solidus 560 °C1040 °F
Liquidus 670 °C1240 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.9 - 95.4 %91.9 - 95.4 %As remainder
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 1.8 - 2.5 %1.8 - 2.5 %
Iron, Fe <= 0.30 %<= 0.30 %
Lithium, Li 1.7 - 2.3 %1.7 - 2.3 %
Magnesium, Mg 1.1 - 1.9 %1.1 - 1.9 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.20 %<= 0.20 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.25 %<= 0.25 %
Zirconium, Zr 0.04 - 0.16 %0.04 - 0.16 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2090-T86
Aluminum 2090-T84
2111 Aluminum Composition Spec
Aluminum 2091-T8x, 10% cold work
Aluminum 8090-T8x

MA2091T8 / 8900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.