MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP615 Melamine Phenolic Paper Laminate Sheet
Categories: Polymer; Thermoset

Material Notes: Room temperature punching and shearing grade up to 0.125 in. thick. NP615 is more flexible with lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated surfaces to give the resulting laminate better arc resistance. Intended for applications where electrical and moisture requirements are secondary.

Information provided by Norplex-Micarta

Key Words: Paper, Melamine, Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/cc
@Thickness 12.7 mm
ASTM D792
Moisture Absorption 3.00 %
@Thickness 1.57 mm
ASTM D570 Condition A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 89
@Thickness 6.35 mm
ASTM D785
Tensile Strength 8400 psi
@Thickness 3.17 mm
CrossWise; ASTM D638 Condition A
 12500 psi
@Thickness 3.17 mm
LengthWise; ASTM D638 Condition A
Flexural Strength 14000 psi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 20000 psi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Flexural Modulus 1000 ksi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 1200 ksi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Compressive Strength 18000 psi
@Thickness 12.7 mm
Flatwise; ASTM D695 Condition A
Shear Strength 11800 psi
@Thickness 1.57 mm
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched 0.570 ft-lb/in
@Thickness 12.7 mm
CrossWise; ASTM D256 Condition E-48/50
 0.590 ft-lb/in
@Thickness 12.7 mm
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.49
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Dielectric Strength 700 V/mil
@Thickness 1.57 mm
ASTM D149 Condition A
Dielectric Breakdown 10000 V
@Thickness 1.57 mm
ASTM D149 Condition D-48/50
 55000 V
@Thickness 1.57 mm
ASTM D149 Condition A
Dissipation Factor 0.096
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Arc Resistance 110 sec
@Thickness 3.17 mm
ASTM D495 Conition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 120 °CUL Bulletin 746b
UL RTI, Mechanical with Impact 120 °CUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
 
Descriptive Properties
Bonding Strength1400[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek TS-102 Thermoset Electrical Insulation Product (Nema Grade: X)
Phillips 66 Syncon® 100 Synthetic R&O Oil
Norplex-Micarta NP615 Phenolic/Melamine Paper Laminate Sheet
Norplex-Micarta NP602 Phenolic Paper Laminate Sheet
Norplex-Micarta MC603 Paper Base Laminate

PNORPM073 / 192830

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.