MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Dow™ DGDC-2100 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DGDC-2100 NT 7 HDPE resin is a high-molecular weight, high density film grade resin. This product was specifically designed to offer an optimal balance of physical properties and processability. DGDC-2100 NT 7 HDPE resin is ideally suited for use in making grocery sacks, consumer and institutional liners, and merchandise bags.
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU, No 10/2011. Consult the regulations for complete details.

Availability: Asia Pacific; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520© 3.2; HPFB (Canada) No Objection; EU, No 10/2011

Form: Pellets

Processing Method: Blown Film; Profile Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Melt Flow  0.070 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.070 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 29.8 N
@Thickness 0.0127 mm
6.70 lb (f)
@Thickness 0.000500 in
Film Tensile Strength at Yield, MD 42.3 MPa
@Thickness 0.0127 mm
6140 psi
@Thickness 0.000500 in
ASTM D882
Film Tensile Strength at Yield, TD 31.8 MPa
@Thickness 0.0127 mm
4610 psi
@Thickness 0.000500 in
ASTM D882
Film Elongation at Break, MD 330 %
@Thickness 0.0127 mm
330 %
@Thickness 0.000500 in
ASTM D882
Film Elongation at Break, TD 410 %
@Thickness 0.0127 mm
410 %
@Thickness 0.000500 in
ASTM D882
2% Secant Modulus  0.965 GPa
@Thickness 0.0127 mm
140 ksi
@Thickness 0.000500 in
MD; ASTM D882
 1.10 GPa
@Thickness 0.0127 mm
159 ksi
@Thickness 0.000500 in
TD; ASTM D882
Puncture Energy 0.893 J
@Thickness 0.0127 mm
0.658 ft-lb
@Thickness 0.000500 in
Elmendorf Tear Strength MD 11 g11 gASTM D1922
Elmendorf Tear Strength TD 73 g73 g0.0005; ASTM D1922
Dart Drop Test 350 g
@Thickness 0.0127 mm
0.772 lb
@Thickness 0.000500 in
ASTM D1709A
Film Tensile Strength at Break, MD 93.8 MPa
@Thickness 0.0127 mm
13600 psi
@Thickness 0.000500 in
ASTM D882
Film Tensile Strength at Break, TD 68.9 MPa
@Thickness 0.0127 mm
9990 psi
@Thickness 0.000500 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C262 °F
 
Optical PropertiesMetricEnglishComments
Haze 69 %
@Thickness 0.0127 mm
69 %
@Thickness 0.000500 in
ASTM D1003
Gloss 9.0 %
@Thickness 0.0127 mm
9.0 %
@Thickness 0.000500 in
45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 °C410 °FExtrusion
Blow-up Ratio (BUR) 4.04.0
 
Descriptive Properties
Film Puncture Resistance128 ft-lb/in30.5 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF440 / 311133

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.