Nylene 5130 PT15 is a low wear 30% glass fiber reinforced nylon 6/6 using Nylene 5130 PT15 provides a low friction and very low wear surface while maintaining the high strength and stiffness required from a glass fiber reinforced material. 5130 PT15 is suitable for applications such as bushings and bearings, wear plates, and other parts where high strength with maximum wear resistance is required. Testing conducted on dry as molded specimen Information provided by Nylene® Global Polymer Solutions. |