MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9057MP Hi-Performance Acrylic 200MP
Categories: Polymer; Adhesive

Material Notes: This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materials. It features exceptional shear strength and adhesion to high surface energy (HSE) plastics and metal surfaces.

The 90xx series of products has a layflat liner on each side which improves die-cutting and handling of intricate die-cut parts.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milAdhesive
 50.8 microns2.00 milAdhesive
 76.2 microns3.00 milPolyester
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 0.455 MPa66.0 psiCohesion Dynamic, PET/Polycarbonate; ASTM D1002
 0.545 MPa79.0 psiCohesion Dynamic, PET/Stainless Steel; ASTM D1002
Peel Strength 0.40538 kN/m2.3125 pli90° Peel, PET/PET, Initial (20 mins); ASTM D3330
 0.44921 kN/m2.5625 pli90° Peel, PET/Polycarbonate, Initial (20 mins); ASTM D3330
 0.5916 kN/m3.375 pli90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330
 0.657 kN/m3.75 pli90° Peel, PET/PET, 72 hrs at RT; ASTM D3330
 0.7231 kN/m4.125 pli90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330
 0.7231 kN/m4.125 pli90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330
 0.789 kN/m4.50 pli90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330
 0.79981 kN/m4.5625 pli90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330
 1.0408 kN/m5.9375 pli90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330
 1.49 kN/m8.50 pli90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330
 1.62 kN/m9.25 pli90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330
 1.6763 kN/m9.5625 pli90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.30e+15 ohm-cm1.30e+15 ohm-cmASTM D257
Surface Resistance >= 5.60e+16 ohm>= 5.60e+16 ohmASTM D257
Insulation Resistance 1.10e+13 ohm1.10e+13 ohm100VDC, 60 sec; Mil-I-46058C
Dielectric Constant 3.333.33ASTM D150
Dielectric Strength 66.9 kV/mm1700 kV/inASTM D149
Dissipation Factor 0.0130.013ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.40 µm/m-°C
@Temperature 27.0 - 175 °C
3.00 µin/in-°F
@Temperature 80.6 - 347 °F
ASTM D696
 
Descriptive Properties
Adhesive Type200MP
Liner94# PCK 7.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33315 / 168062

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.