MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Duratron® U2300 PEI Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 30% Glass Fiber

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Water Absorption 0.18 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.90 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 114ASTM D785
Hardness, Rockwell R 127ASTM D785
Hardness, Shore D 86ASTM D2240
Tensile Strength 17000 psiASTM D638
Tensile Strength at 150°C (300°F) 12500 psiASTM D638
Tensile Strength at 65°C (150°F) 15000 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Tensile Modulus 800 ksiASTM D638
Flexural Strength 27000 psiASTM D790
Flexural Modulus 850 ksiASTM D790
Compressive Strength 32000 psi10% Def.; ASTM D695
Compressive Modulus 625000 psiASTM D695
Izod Impact, Notched 1.00 ft-lb/inASTM D256 Type A
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 770 V/milShort Term; ASTM D149
Dissipation Factor 0.0015
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Thermal Conductivity 1.56 BTU-in/hr-ft²-°FASTM F433
Maximum Service Temperature, Air 340 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 410 °FASTM D648
Glass Transition Temp, Tg 410 °FASTM D3418
Flammability, UL94 V-0
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Conductive / Static Dissipative No
Continuous Sunlight Acceptable
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Limited
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
Machinability71-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Duratron® U1000 PEI Extruded Unfilled Polyetherimide (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide
Mitsubishi Chemical Advanced Materials Duratron® U2100 PEI Extruded 10% Glass Reinforced Polyetherimide
Mitsubishi Chemical Advanced Materials Duratron® T4203 PAI Extruded Polyamide-imide (ASTM Product Data Sheet)
Ensinger Tecapeek® Polyetheretherketone (PEEK)

P1SM51 / 20147

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.