MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Momentive Performance Materials FQE 307U Heat Cured Rubber (HCR), Fluorosilicone base compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: FQE 307U fluorosilicone is a base compound to be considered for applications exposed to non-polar fluids and solvents including fuels, oils and greases. This material typically exhibits the combination of excellent compression set with high tensile strength and elongation at break at low density.

Features: Excellent fuel and oil resistance, Excellent heat resistance, Good physical properties, Very low compression set. FQE 307U fluorosilicone is an excellent candidate to consider for applications like: O-Rings, Dynamic valves, Diaphragms, Seals and gaskets in contact with fuels, oils or greases.

Formulation as tested: 100 pbw FQE 307U fluorosilicone with 0.8 pbw 2,5-dimethyl-2,5-di(tertbutylperoxy)hexane (50%). Vulcanization conditions: 10min/170 °C, post-curing: 4h/200 °C in hot air. Using other peroxides might result in different mechanical properties.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³Uncured; JIS K 6249
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070JIS K 6249
 7171After heat aging 70h/225°C
Tensile Strength 8.50 MPa1230 psiAfter heat aging 70h/225°C
 10.5 MPa1520 psiJIS K 6249
Elongation at Break 198 %198 %After heat aging 70h/225°C
 260 %260 %JIS K 6249
Tear Strength 14.0 kN/m80.1 pliJIS K 6252 Crescent
 18.0 kN/m103 pliDie B.; ASTM D 624
Compression Set 5.0 %
@Temperature 180 °C,
Time 79200 sec
5.0 %
@Temperature 356 °F,
Time 22.0 hour
JIS K 6249
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 °C
@Time 601 sec
338 °F
@Time 0.167 hour
plus 4h at 200ºC post cure vulcanization; as tested. Die B
 
Descriptive Properties
AppearanceOpaque SolidUncured
Plasticity350JIS K 6249. Uncured.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9966 / 265781

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.