MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution Terblend® N 3158 ASA / PA, 9% Mineral filled  (discontinued **)
Categories: Polymer; Thermoplastic; ASA Polymer; Nylon (Polyamide PA)

Material Notes: Terblend® N 3158 is an 9% mineral-filled ABS/PA blend with good dimensional stability, enhanced rigidity and excellent heat resistance, so that this grade can be applied for online-painting.
  • High dimensional stability
  • High rigidity
  • Excellent heat resistance for online-painting
  • Mineral filled (9%)

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Moisture Absorption at Equilibrium 1.3 %
@Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage 0.011 - 0.014 in/inISO 294-4
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 280 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPaISO 527
Elongation at Break 10 %ISO 527
Elongation at Yield 3.0 %ISO 527
Tensile Modulus 2900 MPaISO 527
Flexural Strength 88.0 MPaISO 178
Flexural Modulus 3000 MPaISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 160 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dissipation Factor 0.0075
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 132 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CISO 75
Vicat Softening Point 160 °C
@Load 5.10 kg
50°C/h; ISO 306
 245 °C
@Load 1.02 kg
50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °CISO 294
Mold Temperature 80.0 °CISO 294
Injection Velocity 40.0 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Conditioned)
INEOS Styrolution NAS® 90 Styrene Methyl Methacrylate (SMMA)
INEOS Styrolution NAS® 36 Styrene Methyl Methacrylate (SMMA)
INEOS Styrolution NAS® 30 Styrene Methyl Methacrylate (SMMA)
INEOS Styrolution Luran® S KR2866C ASA / PC

PBASF9048B / 159695

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.