MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Americas Styrenics MC3700 High Heat Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Product Characteristics
  • Easy filling of thin-walled parts
  • Exceptional mold release
  • Improved cycle times in hard to fill parts
  • Food Contact Compliant
  • UL Classification 94HB
  • USP Class VI

Typical Applications

  • Color concentrate carrier
  • Consumer containers, vials, jars, etc.
  • Disposable cutlery
  • Injection molded drink cups

Information provided by AmericasStyrenics LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 in/inASTM D955
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 109ASTM D785
Tensile Strength at Break 6000 psiASTM D638
Tensile Strength 6000 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Tensile Modulus 460 ksiASTM D638
Flexural Strength 7400 psiASTM D790
Flexural Modulus 480 ksiASTM D790
Izod Impact, Notched 0.400 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 181 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 171 °FASTM D648
Vicat Softening Point 201 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips MC3700 High Flow Crystal Polystyrene
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene
Americas Styrenics MB3150 High Heat Crystal Polystyrene

PAMERI905 / 131172

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.