MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® Terra DD18 PA1012  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: VESTAMID® Terra DD is partly based on renewable raw materials and in general has the highest performance of all the bio-based polyamides. VESTAMID® Terra DD is the polycondensation product of 1,10-decamethylene diamine (D) and 1,12-dodecanedioic acid (D). The 1,12-dodecanedioic acid (D) is typically sourced from a petroleum production route, but can also be sourced via palm kernel oil. Because both monomers can be derived from plant oils, VESTAMID® Terra DD is a material that is based 45% to 100% on natural resources. VESTAMID® Terra DD depicts 1,12-dodecanedioic acid from fossil resources, where as DD-G depicts the monomer from biomass resources. Technically speaking, VESTAMID® Terra DD is similar to other high-performance long-chain polyamides such as PA 12 and PA 11. It shows a very high impact strength and heat resistance. Due to its semi-crystalline morphology, VESTAMID Terra DD provides an excellent chemical resistance, e.g., against greases, oils, fuels and hydraulic fluids. It is the best choice in applications where stiffness and impact strength are required.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Water Absorption 1.6 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPaISO 527
Elongation at Break >= 50 %ISO 527
Elongation at Yield 5.0 %ISO 527
Tensile Modulus 1300 MPaISO 527
Charpy Impact Unnotched NB23; ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 16.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 190 °CISO 1183
Vicat Softening Point 154 °C
@Load 5.10 kg
Method B; ISO 306
Glass Transition Temp, Tg 35.0 °CIOS 1183

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® Terra DD22 PA1012
Evonik VESTAMID® Terra DD18-GF30 PA1012
EMS-Grivory Grilamid® L 25 W 40 X PA12-I
EMS-Grivory Grilamid® LBV-30H FWA nat PA12-GF30
Evonik Vestamid® Terra DD16 Nylon 1012

PEVONIL490 / 196694

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.