MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Persian Gulf Polymer PP-EP440L Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: EP440L is a medium flow heterophasic polypropylene copolymer with improved mechanical properties, balance transparency, high gloss and exhibits good antistatic properties. EP440L" is mainly designed for transparent house wares and quality packaging applications. It is an outstanding grade for injection molded containers and thin-walled packaging where clarity is of utmost importance. In many of these applications, "RP340N" can replace PS since it can match the optical properties whilst adding low weight, low odor transfer, chemical resistance and impact strength. Processing Method: Injection molding. Features: High Impact strength, excellent transparency. Typical Applications: Packaging, automotive and consumer goods industries, Luggage, paint pails, buckets, containers, crates, batteries and large toys.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ISO 868
Tensile Strength, Yield 26.0 MPaASTM D638
Elongation at Yield 9.0 %ASTM D638
Flexural Modulus 1400 MPaASTM D790
Izod Impact, Notched 70.0 J/m
@Temperature -20.0 °C
ASTM D256
 170 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CASTM D648
Vicat Softening Point 152 °C
@Load 1.02 kg
ASTM D1525
 
Descriptive Properties
Accelerated Oven Aging360 hrsIn air @ 150°C. ASTM D3012

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERSI980 / 250384

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.