MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

FKuR Kunststoff Terralene® HD 3400 Biobased Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Extrusion Blow Molding. Used in bottles, cans

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³ISO 1183
Melt Flow 19 - 21 g/10 min
@Load 21.6 kg,
Temperature 190 °C
19 - 21 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 27.0 MPa3920 psiISO 527
Tensile Strength, Yield 27.0 MPa3920 psiISO 527
Tensile Modulus 0.875 GPa127 ksiISO 527
Charpy Impact, Notched 3.82 J/cm²18.2 ft-lb/in²ISO 179-1/1 eA
 
Descriptive Properties
Bio-based carbon content (%)95ASTM D 6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUTENE-H ME9180 HDPE
ICO Polymers ICOFLO™ 510-5007 1200 Micron HDPE Powder
NOVA Chemicals SCLAIR® 2712CC HDPE Injection Molding Resin
Formosa Plastics Formolene® E602 Pipe HDPE
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE

PFKUR923 / 192725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.