Notes: Sarlink EE-2268DN is a medium impact, modified polypropylene used in transportation applications. This grade can be processed by extrusion or injection molding. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Filled; High Hardness; Light Stabilized; Low Flow; Medium Density; Sunlight Resistant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; General Purpose RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion: Injection Molding Information provided by Teknor Apex |