MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ STAT-KON™ EX01696C PEI (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP STAT-KON EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 94.0 MPa13600 psiASTM D638
Elongation at Break 3.6 %3.6 %ASTM D638
Flexural Strength 158 MPa22900 psiASTM D790
Flexural Modulus 3.63 GPa526 ksiISO 178/1A
Izod Impact, Notched 0.370 J/cm0.693 ft-lb/inASTM D256
Izod Impact, Unnotched 4.80 J/cm8.99 ft-lb/inASTM D4812
Tangent Modulus 3690 MPa535000 psi50 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+6 - 1.00e+8 ohm1.00e+6 - 1.00e+8 ohmASTM D257
 
Processing PropertiesMetricEnglishComments
Zone 1 345 - 355 °C653 - 671 °F
Zone 2 355 - 365 °C671 - 689 °F
Zone 3 365 - 375 °C689 - 707 °F
Melt Temperature 360 - 365 °C680 - 689 °F
Mold Temperature 120 - 150 °C248 - 302 °F
Drying Temperature 120 - 150 °C248 - 302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Screw Speed 60 - 100 rpm60 - 100 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI22200 / 215336

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.