MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 62 Shore A  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene

Material Notes: Styrene-Butadiene Copolymer

Description: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 602 provides good fluidity properties to the compound while keeping good mechanical properties.

Applications: Thanks to it very high crumb porosity Finaprene® 602 is designed for the compounding industry. This crumb shape, along with the broad molecular weight distribution confer a quick oil absorption to the polymer and lead to the production of fluid compounds. This fluidity will enhance the surface aspect of the injected article. The structure of 602 is n = 2, 3, 4, 5.

Content of the compound for which the listed properties apply:
F484: 0
F435: 45
F411x: 30
F602: 25
F507: 10
GPPS: 40
HIPS: 10
Oil: 60
CaCO3: 15

Additional Notes:
DIN Abrasion: 175 mm³

Data provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9852 g/cc0.03559 lb/in³Finaprene 2602 Test
Melt Flow 38 g/10 min
@Load 5.00 kg,
Temperature 190 °C
38 g/10 min
@Load 11.0 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262Finaprene 1505 Test
Tensile Strength, Ultimate 5.60 MPa812 psiASTM D638
Elongation at Break 414 %414 %ASTM D638
300% Modulus 5.00 MPa
@Strain 300 %
725 psi
@Strain 300 %
Tear Strength 29.4 kN/m168 pli
Abrasion 175175mm³; DIN Abrasion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFINAP026 / 38613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.