MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik BREAK-THRU® EM O 7 Surfactants
Categories: Fluid

Material Notes: Product description: Oleic acid polyglycol ester

Application: BREAK-THRU® EM O 7 is a non-ionic, oil-soluble emulsifier for mineral oils, vegetable oils, methyl or ethyl esters of fatty acids, and solvents. It is clear to slightly hazy in mineral oils, methyl or ethyl esters of fatty acids, and fatty oils. BREAK-THRU® EM O 7 is specifically designed for use as an oil in water emulsifier for pesticides. A recommended dose rate is about 1-10 wt. % for mineral oils, and 5-10 wt% for vegetable and methylated vegetable oils.

Properties & Benefits: BREAK-THRU® EM O 7 is an environmentally acceptable emulsifier for mineral and paraffinic oils with reduced foam and can be used as an alternative to Nonyl-phenol Ethoxylate surfactants(NPEs) in a variety of applications. BREAK-THRU® EM O 7 conforms to use as a pesticide inert ingredient pre- and post-harvest under FIFRA 40 CFR 180.910.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 - 1.01 g/cc
pH 6.0 - 8.0
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 6.0
 
Descriptive Properties
Appearanceyellow, clear liquid
Content10.4HLB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL699 / 196903

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.