MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling LAMIGAMID® 400 Cast Polyamide 6, Elastomer Modified, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Application: gear-wheels, chain-wheels, hydrocyclones, housings, outrigger floats

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: RIM-PA 6 G
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO R 1183
Moisture Absorption at Equilibrium 2.3 %DIN 53473
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness <= 100 MPaHc 30; ISO 2039; partially
Tensile Strength, Yield 45.0 - 60.0 MPaISO-DIS 527
Tensile Modulus >= 1300 MPaDIN 53457
Flexural Strength <= 50.0 MPaDIN 54352
Flexural Modulus <= 2000 MPaDIN 53457
Izod Impact, Notched (ISO) >= 1.00 J/cm²ISO 180-1A
Izod Impact Resistance NBswinging hammer 0,1 DIN 51222; DIN 53453
Tear Strength Test >= 0.45ISO-DIS 527
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 - 150 µm/m-°C
@Temperature 20.0 - 100 °C
DIN 53752
Melting Point 210 - 218 °CISO R 1218
Maximum Service Temperature, Air 80.0 °CContinuous
Deflection Temperature at 0.46 MPa (66 psi) 180 - 195 °CV-notch; ISO R 75
Minimum Service Temperature, Air -40.0 °CContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brueggemann Chemical Nyrim® 1000 (Dry)
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber
Brueggemann Chemical Nyrim® 1000 (Conditioned)
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)
CoorsTek RB B4C Reaction-Bonded Boron Carbide

PSCHW025 / 90222

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.