MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Schott FITC A-40 Fluorescence Bandpass Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Standard filter for fluorescence Microscopy or fluorescence spectroscopy. Steeper filters are also available. Fluorochrome FITC (fluorescein-isothiocyanate) is used in fluorescence microscopy and spectroscopy for investigating immune reactions. These filters separate the absorbed light from the light source (FITC A-40) and the emitted light from the sample under investigation (FITC E-45).

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness <= 350 microns
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °Ccontinuous
 100 °Cintermittent
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 0.010 %
@Wavelength <=430 nm
 >= 0.010 %
@Wavelength 515 - 740 nm
 <= 75 %
@Wavelength 460 - 480 nm
IR Transmittance >= 0.010 %
@Wavelength 740 - 850 nm
 
Descriptive Properties
Edge wavelengths445-455 nm
 487-497 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott SF57HT 847238.551, Optical Glass
Schott RS 520 Radiation Shielding Glass
Schott B270™ Sheet Glass
Möller Medical NanoSkin 78 NanoCoating
Esstech V-116-1130 Barium Silicate Glass

CSGT9817 / 183070

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.