MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omni Plastics OmniLon™ PA6/6 MF40 Nylon 6/6, 40% Mineral reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: 40% Mineral reinforced; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Filler Content 40 %ASTM D2584
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 90.0 MPaASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Strength 162 MPaASTM D790
Flexural Modulus 6895 MPaASTM D790
Izod Impact, Notched 37.0 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
@Thickness 3.17 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 520 - 560 °F
Middle Barrel Temperature 520 - 560 °F
Front Barrel Temperature 520 - 560 °F
Nozzle Temperature 520 - 580 °F
Melt Temperature 520 - 560 °F
Mold Temperature 80.0 - 140 °F
Drying Temperature 180 °F
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.20 %
Back Pressure 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® N-265 NF3001 40% Mineral Filled PA66 (Dry)
Celanese Minlon® 10B40 NC010 PA66-MD40
Nylene® PA6/6 Mineral Filled 6140 HS Nylon 6/6
Nylene® PA6/6 Mineral Filled 6440 HS Nylon 6/6
Omni Plastics OmniLon™ 6/6 PA6/6 MF40 Mineral Filled Nylon

POMNI5019 / 185165

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.