SAERfoam is a structural hybrid core material with 3D glass bridges. SAERfoam can replace conventional core materials such as PVC, PET and balsa in an innovative manner: Ultralight foam (PU/PE/PIR) is combined with 3D glass reinforcements.Information provided by SAERTEX®. |