MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ B-536 Adhesive System
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties:
  • Very high strength bonding of dissimilar materials.
  • High moisture and solvent resistance.
  • Fast ambient cure with good pot life.
  • Ease of use.

Applications: Outstanding adhesive for very high strength potting and assembly applications. Bonds most plastics, metals, glass and ceramics. Good for electronics applications. High moisture resistance. Full cure 60 minutes at ambient or 10 minutes at 170º F or higher temperatures for faster cure down to 15 sec.

Key Words: Epoxy Adhesive, Sealant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 2500 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7418 psiAmbient Cure
Tensile Strength, Ultimate 7693 psiPeak; Ambient Cure
Tensile Strength, Yield 7693 psiAmbient Cure
Elongation at Break 9.2 %Ambient Cure
Elongation at Yield 8.6 %Ambient Cure
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 minAmbient
Pot Life 45 minAmbient
 
Descriptive Properties
ColorClear with slight amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAQREL01 / 24217

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.