MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elmet Technologies Pure Tungsten Wire
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy; Pure Element

Material Notes: The chemical composition complies with ASTM requirements for powder lot analysis. Actual finished part chemical analysis and mechanical properties are not routinely evaluated per ASTM requirements. ASTM specifications and test methods are used as guidelines to control and monitor production processes to assure product quality. Applicable ASTM Material Standards: Rod/Wire – F288-96 (re-approved 2002). This product meets the requirements of low copper and mercury-free materials.

Information provided by Elmet Technologies.

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density >= 19.3 g/cc
a Lattice Constant 3.1585 Å
Vapor Pressure 1.93e-15 torr
@Temperature 1527 °C
 7.90e-9 torr
@Temperature 2127 °C
 3.99e-8 torr
@Temperature 2000 °C
 0.00000500 torr
@Temperature 2500 °C
 0.0000650 torr
@Temperature 2727 °C
 0.000997 torr
@Temperature 3000 °C
 0.00468 torr
@Temperature 3227 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 183.92
Atomic Number 74
Atomic Volume 9.53[cc/gm atom]
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 59000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000550 ohm-cm
@Temperature 20.0 °C
 0.00000728 ohm-cm
@Temperature 100 °C
 0.0000180 ohm-cm
@Temperature 500 °C
 0.00002243 ohm-cm
@Temperature 700 °C
 0.0000330 ohm-cm
@Temperature 1000 °C
 0.00003465 ohm-cm
@Temperature 1100 °C
 0.00004966 ohm-cm
@Temperature 1500 °C
 0.00005752 ohm-cm
@Temperature 1800 °C
 0.00006961 ohm-cm
@Temperature 2100 °C
 0.00100 ohm-cm
@Temperature 3000 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.45 µm/m-°C
@Temperature 0.000 - 500 °C
Annealed
 4.98 µm/m-°C
@Temperature 0.000 - 500 °C
worked
Specific Heat Capacity 0.140 J/g-°C
Thermal Conductivity 0.222 cal cm/sec-cm²-°C
@Temperature 2000 °C
 0.245 cal cm/sec-cm²-°C
@Temperature 1727 °C
 0.253 cal cm/sec-cm²-°C
@Temperature 1527 °C
 0.260 cal cm/sec-cm²-°C
@Temperature 1327 °C
 0.268 cal cm/sec-cm²-°C
@Temperature 1127 °C
 0.275 cal cm/sec-cm²-°C
@Temperature 927 °C
 0.290 cal cm/sec-cm²-°C
@Temperature 500 °C
 0.380 cal cm/sec-cm²-°C
@Temperature 100 °C
 0.400 cal cm/sec-cm²-°C
@Temperature 20.0 °C
Melting Point 3410 °C
Boiling Point 5900 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0025 %
Carbon, C <= 0.0050 %
Chromium, Cr <= 0.0020 %
Copper, Cu <= 0.0010 %
Iron, Fe <= 0.0030 %
Molybdenum, Mo <= 0.0050 %
Nickel, Ni <= 0.0030 %
Other, each <= 0.0020 %
Oxygen, O <= 0.0050 %
Potassium, K <= 0.0020 %
Silicon, Si <= 0.0040 %
Sodium, Na <= 0.0020 %
Tungsten, W >= 99.95 %
 
Descriptive Properties
Electron Work Function4.55
Lattice StructureBody Centered Cubic
RoHS Compliance2002/95/EC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NELMET933 / 242054

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.