MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polikim EFALON® B-60 PTFE, 60% Bronze Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearings, piston rings, valve sets, valve components.

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.80 - 4.00 g/ccASTM D792
Deformation 1.0 - 1.1 %
@Temperature 150 °C,
Time 86400 sec,
Pressure 0.981 MPa
total
 1.5 - 2.0 %
@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
permanent; ASTM D621
 3.7 - 4.8 %
@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
total; ASTM D621
 9.0 - 10 %
@Temperature 150 °C,
Time 86400 sec,
Pressure 4.90 MPa
total
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65 - 70ASTM D2240
Tensile Strength, Ultimate 140 - 220 kg(f)/cm²ASTM D638
Elongation at Break 110 - 220 %ASTM D638
Compressive Strength 105 - 110 kg(f)/cm²1% Deformation; ASTM D695
Izod Impact, Notched (ISO) 10.0 - 11.0 kJ/m²ASTM D256
Coefficient of Friction 0.13
Coefficient of Friction, Static 0.070
Limiting Pressure Velocity 0.004905 - 0.005232 MPa-m/sec3 m/min
 0.00638 - 0.00654 MPa-m/sec30 m/min
 0.00736 - 0.00900 MPa-m/sec300 m/min
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+7 ohm-cmASTM D257
Surface Resistance >= 1.00e+9 ohm50% rel. humidity; ASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 75.0 - 90.0 µm/m-°C
@Temperature 25.0 - 100 °C
ASTM D696
 100 - 115 µm/m-°C
@Temperature 25.0 - 200 °C
ASTM D696
 130 - 140 µm/m-°C
@Temperature 25.0 - 300 °C
ASTM D696
Thermal Conductivity 0.00170 - 0.00200 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 270 °Ccontinuous
Minimum Service Temperature, Air -260 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® PB3060 60% Bronze, PTFE Filled Compound
Fluorseals PTFE 60% bronze filled
Trelleborg Sealing Solutions Turcite® TA Self-Lubricating Thermoplastic Rod
Adamas Adalon® 817 PTFE, 60% Bronze
AGC FC 146 PTFE, 60% Bronze

PPOLIK007 / 99817

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.