MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Features

Determined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent flow of the material predetermines it for the manufacturing of complicated small and large surface mouldings. Possible use for products with wall thickness from 0.5 mm. High grade brightness also at coloured types. Delivered in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA6/66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³
Viscosity Measurement 0.75 - 0.870.75 - 0.87
Linear Mold Shrinkage 0.0075 cm/cm0.0075 in/in
Linear Mold Shrinkage, Transverse 0.0087 cm/cm0.0087 in/in
Melt Flow 10 g/10 min
@Load 0.325 kg,
Temperature 270 °C
10 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi
Elongation at Break 6.0 %6.0 %
Tensile Modulus 3.65 GPa529 ksi
Flexural Strength 125 MPa18100 psi
Flexural Modulus 3.30 GPa479 ksi
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -20.0 °C
38.1 ft-lb/in²
@Temperature -4.00 °F
 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.300 J/cm²
@Temperature -20.0 °C
1.43 ft-lb/in²
@Temperature -4.00 °F
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm
Surface Resistance 1.00e+12 ohm1.00e+12 ohm
Dielectric Strength 25.0 kV/mm635 kV/in
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °F
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °F
Vicat Softening Point 215 °C419 °FB
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Glow Wire Test 960 °C1760 °Fat 3 mm
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 3008 Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade
CENTROPLAST CENTROMID 6.6 Polyamide 6.6

PPLACO383 / 121007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.