MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Plastics Kynar® 2850 PVDF Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: KYNAR polyvinylidene fluoride is a tough engineering thermoplastic that offers a unique balance of performance properties. It has the characteristic stability of fluoropolymers when exposed to harsh thermal, chemical and ultraviolet environments. KYNAR is also inherently UV stable, mechanically tough, abrasion and flame resistant. Resin meets the requirements of FDA, USDA, USP VI, Dairymen 3A, UL V-0, FM 4910

Applications include:

  • Semiconductor Packaging, Process and Testing Components
  • Semiconductor Wet Processing Components
  • Chemical Process/Storage tanks
  • Chemical tank liners
  • Fire Safety Components
  • DI Water System Components
  • Electrical Insulating Components
  • Radiation Barriers

Kynar® is a trademark of Arkema Group. Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 g/ccASTM D792
Water Absorption 0.040 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70 - 75ASTM D2240
Tensile Strength, Yield 4500 - 6000 psiASTM D638
Elongation at Break 200 %ASTM D638
Elongation at Yield 10 - 20 %ASTM D638
Tensile Modulus 150000 - 220000 psiASTM D638
Flexural Strength 3000 - 5000 psiASTM D790
Flexural Modulus 150000 - 180000 psiASTM D790
Izod Impact, Notched 2.00 - 8.00 ft-lb/inASTM D256
Izod Impact, Unnotched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cmASTM D257
Dielectric Constant 3.5 - 10.2
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µin/in-°FASTM D696
Melting Point 311 - 320 °FASTM D4591
Maximum Service Temperature, Air 240 °FContinuous Use
Deflection Temperature at 0.46 MPa (66 psi) 140 - 167 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 - 131 °FASTM D648
Flammability, UL94 V-0
Oxygen Index 43 %ASTM D2868
 
Compliance PropertiesOriginal ValueComments
3A-Dairy Yes
FDA Yes
USDA Yes
USP Class VI Yes
 
Descriptive Properties
ColorNatural Beige, Black, Red

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Kynar Flex® 2850 WR PVDF
Omnia Plastica Kynar® PVDF
Techmer ES HiFill® TPX-PVDF-03009 C
Arkema KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding

PWEST142 / 72761

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.