MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
The Chemical Company VESTINOL® 9 Diisononyl Phthalate, C6H4(COOC9H19)2
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Diisononyl Phthalate (DINP) C6H4(COOC9H19)2, is a clear, colorless, and almost odorless liquid chemical. It is soluble in most organic solvents. DINP is primarily used as a PVC plasticizer. As compared to DOP, the low volatility and better endurability of DINP significantly reduces the fume emissions during the processing procedure and improves its permanence in the final product. DINP is a mixture of isomers that have alkyl chains from 7 to 9 carbons long, but the largest portion of the mixture have chains composed of 8-carbon in length (a.k.a. isononyl alcohol). DINP is a general purpose plasticizer with a broad range of applications used in flexible PVC. It is widely used in the toy, construction, and general consumer product markets. It has limited use in food packaging and is not used in medical applications.

Information provided by The Chemical Company

Key Words: DINP; CAS Number 28553-12-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.972 - 0.977 g/cc
@Temperature 20.0 °C
DIN 51 757/ASTM D4052
Brookfield Viscosity 72 - 82 cP
@Temperature 20.0 °C
DIN S3015/ASTM D445
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.040mg KOH/g; DIN EN ISO 3628/ASTM D1045
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.484 - 1.488DIN 51 423/2/ASTM D1045
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.050 %Percent by mass; DIN 51 777/ASTM E 203
 
Descriptive Properties
AppearanceClear and free of suspended matter
Assay= 99.6%Degussa-Hüls
Hazen Color Value (pt-co)< 40Mg Pt/I, DIN ISO 6271/ASTM D1209

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik ELATUR® CH
Evonik VESTINOL® 9 Plasticizer
Geon® Performance Solutions Synplast™ TINTM-E Triisononyl Trimellitate
BASF Palatinol® N Diisononyl Phthalate

PTCC007 / 106996

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.