MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ND Industries ScrewGrade® 111 Removable Threadlocker
Categories: Polymer; Adhesive; Thermoset

Material Notes: A low strength threadlocker which eliminates vibrational loosening, and seals against leakage and corrosion.

Typical Uses

soft metal fasteners, precision screws, and locking fasteners smaller than .25" in diameter.

Meets military spec MIL-S-46163 Type II Grade M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1200 - 1500 cPThixotropic
 
Mechanical PropertiesOriginal ValueComments
Impact Test 20.0 - 50.0 in-lbPrevail
 50.0 - 100 in-lbBreak
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 minWith Primer (Fixture)
 20.0 minOn steel (fixture)
 24.0 hourWith Primer (Full)
 24.0 hourOn steel (Full)
 
Descriptive Properties
ColorPurple
Gap Fill, in.0.005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® 222MS Low Strength/Small Screw Threadlocker
Overview of materials for Stainless Steel
Chosun Refractories PTA-180 Plastic Refractory

PNDIND00 / 54750

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.