MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Assab Steels 8407 2M Hot Work Steel
Categories: Metal; Ferrous Metal; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by:
  • Good resistance to abrasion at both low and high temperatures.
  • High level of toughness and ductility
  • Uniform and high level of machinability and polishability
  • Good high-temperature strength and resistance to thermal fatigue.
  • Excellent through-hardening properties
  • Very limited distortion during hardening.

Applications: Tools for Extrusion: Dies, backers, die holders, liners, dummy blocks, stems.
Plastic molding applications: Injection molding of thermoplastics: long production runs. Molding of parts in thermosetting plastic with finish requirements.

AISI H13, W.-Nr. 1.2344

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.281 lb/in³
 0.272 lb/in³
@Temperature 800 °C
 0.277 lb/in³
@Temperature 400 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 31holding time 100 hours at 600°C. Austenitizing temperature 1020°C
 43holding time 10 hours at 600°C. Austenitizing temperature 1020°C
 43holding time 100 hours at 550°C. Austenitizing temperature 1020°C
 46tempering temperature 600°C. Austenitizing temperature 1020°C
 51holding time 10 hours at 500°C. Austenitizing temperature 1020°C
 51holding time 10 hours at 550°C. Austenitizing temperature 1020°C
 51holding time 1 hour at 600°C. Austenitizing temperature 1020°C
 48 - 54Hardness before tempering. Austenitizing temperature: 1000°C. Soaking time 45 minutes.
 50 - 56Hardness before tempering. Austenitizing temperature: 1020°C. Soaking time 30 minutes.
 53holding time 10 hours at 500°C tempering temperature
 53holding time 1 hour at 550°C. Austenitizing temperature 1020°C
 54holding time 1 hour at 500°C tempering temperature
 54Taken from tempering graph. At tempering temperature 300°C. Austenitizing temperature 1020°C
Tensile Strength at Break 285 MPa
@Temperature 700 °C
Rm. Austenitizing temp. 1020°C. Tempering temp. 610°C
 930 MPa
@Temperature 550 °C
Rm. Austenitizing temp. 1020°C. Tempering temp. 610°C
Tensile Strength, Ultimate 1420 MPaRm. 45 HRC.
 1820 MPaRm. 52 HRC.
Tensile Strength, Yield 1280 MPaRp02. 45 HRC.
 1520 MPaRp02. 52 HRC.
 150 MPa
@Temperature 700 °C
Rp02
 720 MPa
@Temperature 550 °C
Rp02
Modulus of Elasticity 202.5 GPa
 130 GPa
@Temperature 800 °C
 175 GPa
@Temperature 400 °C
Impact Test 14.0 JDuring tempering at 550°C tempering temperature (2h + 2h)
 20.0 JDuring tempering at 250°C tempering temperature (2h + 2h)
 22.0 JDuring tempering at 650°C tempering temperature (2h + 2h)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.6 µm/m-°C
@Temperature 20.0 - 400 °C
 13.9 µm/m-°C
@Temperature 20.0 - 800 °C
Thermal Conductivity 24.6 W/m-K
@Temperature 20.0 °C
 26.2 W/m-K
@Temperature 400 °C
 27.6 W/m-K
@Temperature 800 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.39 %
Chromium, Cr 5.3 %
Iron, Fe 90.71 %
Manganese, Mn 0.40 %
Molybdenum, Mo 1.3 %
Silicon, Si 1.0 %
Vanadium, V 0.90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Assab Steels 8407 SUPREME Hot Work Steel
AISI 1025 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1023 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 50 mm (2 in.) round
AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 25 mm (1 in.) round

NASSAB15 / 15033

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.