MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® CP-13057G CLR Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-13057G CLR is a very soft clear thermoplastic elastomer gel designed for a variety of consumer product applications. This grade exhibits high flow and is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: High Flow; Low Hardness; Low Density; Low Specific Gravity; Soft: Without Fillers

Uses: Consumer Applications; Safety Equipment; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.870 g/ccASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 125 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8.0
@Time 1.00 sec
Injection Molded; ASTM D2240
Hardness, Shore OO 57
@Time 5.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 272 psi20 in/min, Flow; ASTM D412
 323 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain 14.0 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 23.0 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 25.0 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 60.0 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 790 %20 in/min, Flow; ASTM D412
 2100 %20 in/min, Across Flow; ASTM D412
Tear Strength 32.0 pliFlow; Method Ba, Angle (Unnicked); ASTM D624
 47.0 pliAcross Flow; Method Ba, Angle (Unnicked); ASTM D624
Compression Set 39 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 350 °F
Middle Barrel Temperature 260 - 360 °F
Front Barrel Temperature 270 - 370 °F
Nozzle Temperature 280 - 380 °F
Melt Temperature 280 - 380 °F
Mold Temperature 50.0 - 90.0 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0777 / 237268

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.