MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Supreme SAE 10W-30 Synthetic Motor Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Supreme 100% Synthetic Motor Oils are designed for those drivers who demand the ultimate in engine protection. They provide an extra measure of protection for the investment in a sport utility vehicle (SUV), high performance, or luxury car. Chevron Supreme 100% Synthetic Motor Oils give improved protection to high output, supercharged and turbocharged performance vehicles.

Chevron Supreme 100% Synthetic Motor Oils are formulated using 100% synthetic base stocks for the best performance. The improved volatility and stability of synthetic base stocks give reduced oil consumption, faster engine starting (especially in cold weather), and extremely fast lubrication of all moving parts compared to conventional mineral oils. In addition, a special blend of additives protects the engine against harmful deposits and wear.

SAE 10W-30 is the most widely used viscosity grade in the U.S. It exceeds the requirements and API SJ and ILSAC GF-2.

ApplicationsChevron Supreme Synthetic Motor Oils are recommended for all four-stroke gasoline engines in passenger cars, sprot utility vehicles, and light trucks.

Key Words: CPS Number: 220129; MSDS Number: 7936
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 33.4 °
Viscosity 2100 cP
@Temperature -20.0 °C
Cold Crank
Viscosity Measurement 146Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 66.3 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 10.4 cStASTM D445
Ash 1.11 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 9.2ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -51.0 °CASTM D97
Flash Point 249 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.092 %
Zinc, Zn 0.128 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV036 / 74651

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.