MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos H00M-01 Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Suggested fabrication methods: Extrusion; Thermoforming

Features: High melt strength, High stiffness, Medium-term heat aging

Complies with FDA specification, Title 21, CFR 177.1520.

Typical applications: Thick sheet, Fabricated parts, Strapping

Typical property data below from injection molded samples.

Key Words: High Melt Strength, High Stiffness, Medium-Term Heat Aging
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.886 - 0.926 g/ccASTM D1505
Water Absorption <= 0.010 %24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cmASTM D955
Melt Flow 0.47 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 79 - 108Normal range for injection molding resins; ASTM D785
Tensile Strength, Yield 39.0 MPaASTM D638
Elongation at Break 28 %ASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus 1.70 GPaASTM D790A
Izod Impact, Notched 0.200 - 0.300 J/cm
@Diameter 3.17 mm
bar
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ProcessExtrusion/Thermoforming

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H03G-03 Polypropylene Homopolymer
BP Amoco ACCPRO® 9119X Extrusion Grade Polypropylene
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
BP Amoco ACCPRO® 9644X Injection Grade Polypropylene
Braskem RP 541 Polypropylene

PBPP22 / 27663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.