Vydyne 41H NT is general-purpose, high impact-modified, heat stabilized PA66 resin. The product offers improved resistance to thermal degradation. 41H NT is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline.Information provided by Ascend Performance Materials. |