MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotchcast™ 2130 Flame-Retardant Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 3M Scotchcast Flame-Retardant Compound 2130 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. Its unique formulation makes it particularly suited to withstand the rugged conditions under which mine and portable cables must operate. When used in accordance with the appropriate kit configuration, 2130 Compound conforms to MSHA 30 CFR 18.64. Flame-Retardant 2130 Compound is also used as the insulating material for cable splices operating at up to 1000 volts and designed for 90°C continuous use 130°C overload.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.215 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83ASTM D2240
Tensile Strength at Break 7.45 MPaASTM D412
Elongation at Break 377 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.07
@Frequency 60.0 Hz,
Temperature 23.0 °C
ASTM D150
 5.82
@Frequency 60.0 Hz,
Temperature 60.0 °C
ASTM D150
 6.24
@Frequency 60.0 Hz,
Temperature 90.0 °C
ASTM D150
Dielectric Strength 371 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °CContinuous
 130 °C
Glass Transition Temp, Tg -80.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 - 24.0 hour
@Temperature 21.0 °C
De-Mold Time: 1.5-2 hrs
 24.0 - 30.0 hour
@Temperature 10.0 °C
De-Mold Time: 3.5-4 hrs
 >= 36.0 hour
@Temperature 0.000 °C
De-Mold Time: 6-8 hrs
Gel Time 17.0 min3M Method TM-67
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35238 / 169985

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.