MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nickel Silver, UNS C73500, OS015 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.015 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding; Poor Suitability – Seam Weld, Capacity for Being Hot Formed

Typical uses: Coinage; Fashion jewelry; Flatware; Hollowware; Medallions; Optical goods; Zippers; Name plates

Applicable Specifications: Bar – ASTM B122/B122M; Plate - ASTM B122/B122M; Sheet – ASTM B122/B122M; Strip – ASTM B122/B122M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 393 MPa57000 psi
Tensile Strength, Yield 186 MPa27000 psi0.2% Offset
Tensile Modulus 124 GPa18000 ksi
Modulus of Rigidity 46.9 GPa6800 ksi
Poissons Ratio 0.320.32Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000260 ohm-cm0.0000260 ohm-cm6.5% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 300 °C
8.90 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 3.03 W/m-K21.0 BTU-in/hr-ft²-°F
Melting Point 1091 - 1135 °C1995 - 2075 °F
Solidus 1091 °C1995 °F
Liquidus 1135 °C2075 °F
Annealing Point 538 - 816 °C1000 - 1500 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 70.5 - 73.5 %70.5 - 73.5 %
Iron, Fe <= 0.25 %<= 0.25 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni 16.5 - 19.5 %16.5 - 19.5 %
Zinc, Zn 6.2 - 13 %6.2 - 13 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC73500x5 / 293121

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.