MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Guadua Bamboo
Categories: Wood and Natural Products; Wood

Material Notes: From South America; used in manufactured bamboo products. Relatively coarse grain and relatively large nodes. A modest increase in mechanical properties occurs toward the outside of the plant (the culm wall).

Key Words: Guadua angustifolia; Giant Timber Bamboo
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.650 g/cc0.0235 lb/in³at 12.6% moisture (equilibrium at 65% RH and 20°C)
Moisture Absorption at Equilibrium 12.6 %12.6 %65% RH
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2100 N472 lb (f)Internode; Inside; Janka Hardness
 3000 N674 lb (f)Internode; Outside; Janka Hardness
 3000 N674 lb (f)Node; Inside; Janka Hardness
 3600 N809 lb (f)Node; Outside; Janka Hardness
Modulus of Rupture >= 0.0850 GPa>= 12.3 ksi5th percentile; 4 point bend test
 0.105 GPa15.2 ksiNode; Inside; 4 point bend test
 0.108 GPa15.7 ksiNode; Outside; 4 point bend test
 0.120 GPa17.4 ksiInternode; Inside; 4 point bend test
 0.138 GPa20.0 ksiInternode; Outside; 4 point bend test
Flexural Modulus 12.0 GPa1740 ksiNode; Inside; 4 point bend test
 12.8 GPa1860 ksiNode; Outside; 4 point bend test
 >= 13.2 GPa>= 1910 ksi5th percentile; 4 point bend test
 14.0 GPa2030 ksiInternode; Inside; 4 point bend test
 14.0 GPa2030 ksiInternode; Outside; 4 point bend test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Moso Bamboo
American Red Oak Wood
American Balsa Wood
American White Oak Wood
Tropical Balsa Wood

PTSAV900 / 146103

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.