MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 5052-H38
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: This alloy has good workability, very good corrosion resistance, high fatigue strength, weldability, and moderate strength. This leads to its use in aircraft fuel/oil lines, fuel tanks, other transportation areas, sheet metal work, appliances and lighting, wire, and rivets.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95052; ISO AlMg2.5; Aluminium 5052-H38; AA5052-H38; Al5052-H38
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.68 g/cc0.0968 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7777AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 100100Converted from Brinell Hardness Value
Hardness, Vickers 8787Converted from Brinell Hardness Value
Tensile Strength, Ultimate 290 MPa42000 psiAA; Typical
 234 MPa
@Temperature 149 °C
33900 psi
@Temperature 300 °F
 276 MPa
@Temperature 100 °C
40000 psi
@Temperature 212 °F
 290 MPa
@Temperature -28.0 °C
42100 psi
@Temperature -18.4 °F
 290 MPa
@Temperature 24.0 °C
42100 psi
@Temperature 75.2 °F
 303 MPa
@Temperature -80.0 °C
43900 psi
@Temperature -112 °F
 414 MPa
@Temperature -196 °C
60000 psi
@Temperature -321 °F
Tensile Strength, Yield 255 MPa37000 psiAA; Typical
 193 MPa
@Strain 0.2 %,
Temperature 149 °C
28000 psi
@Strain 0.2 %,
Temperature 300 °F
 248 MPa
@Strain 0.2 %,
Temperature 100 °C
36000 psi
@Strain 0.2 %,
Temperature 212 °F
 255 MPa
@Strain 0.2 %,
Temperature -28.0 °C
37000 psi
@Strain 0.2 %,
Temperature -18.4 °F
 255 MPa
@Strain 0.2 %,
Temperature 24.0 °C
37000 psi
@Strain 0.2 %,
Temperature 75.2 °F
 262 MPa
@Strain 0.2 %,
Temperature -80.0 °C
38000 psi
@Strain 0.2 %,
Temperature -112 °F
 303 MPa
@Strain 0.2 %,
Temperature -196 °C
43900 psi
@Strain 0.2 %,
Temperature -321 °F
Elongation at Break  14 %
@Temperature 24.0 °C
14 %
@Temperature 75.2 °F
 15 %
@Temperature -28.0 °C
15 %
@Temperature -18.4 °F
 16 %
@Temperature 100 °C
16 %
@Temperature 212 °F
 18 %
@Temperature -80.0 °C
18 %
@Temperature -112 °F
 24 %
@Temperature 149 °C
24 %
@Temperature 300 °F
 25 %
@Temperature -196 °C
25 %
@Temperature -321 °F
 7.0 %
@Thickness 1.59 mm
7.0 %
@Thickness 0.0625 in
AA; Typical
 8.0 %
@Diameter 12.7 mm
8.0 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 70.3 GPa10200 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Ultimate Bearing Strength 538 MPa78000 psiEdge distance/pin diameter = 2.0
Bearing Yield Strength 386 MPa56000 psiEdge distance/pin diameter = 2.0
Poissons Ratio 0.330.33
Fatigue Strength 138 MPa
@# of Cycles 5.00e+8
20000 psi
@# of Cycles 5.00e+8
completely reversed stress; RR Moore machine/specimen
Machinability 50 %50 %0-100 Scale of Aluminum Alloys
Shear Modulus 25.9 GPa3760 ksi
Shear Strength 165 MPa24000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000499 ohm-cm
@Temperature 20.0 °C
0.00000499 ohm-cm
@Temperature 68.0 °F
AA; Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  22.1 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.3 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.8 µm/m-°C
@Temperature 20.0 - 200 °C
13.8 µin/in-°F
@Temperature 68.0 - 392 °F
 25.7 µm/m-°C
@Temperature 20.0 - 300 °C
14.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 138 W/m-K960 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 607.2 - 649 °C1125 - 1200 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 607.2 °C1125 °FAA; Typical
Liquidus 649 °C1200 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °Fholding at temperature not required
Hot-Working Temperature 260 - 510 °C500 - 950 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95.7 - 97.7 %95.7 - 97.7 %As remainder
Chromium, Cr 0.15 - 0.35 %0.15 - 0.35 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 2.2 - 2.8 %2.2 - 2.8 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5052-H32
Aluminum 5052-H36
Aluminum 5052-H34
Aluminum 5052-O
Aluminum 5083-H34; 5083-H343

MA5052H38 / 9158

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.