MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 M150 Bearing Oil
Categories: Fluid; Lubricant

Material Notes: Bearing Oil M is a high-quality, rust and oxidation (R&O)-inhibited circulating oil specifically developed for the lubrication of backup roll bearings manufactured by Morgan Construction Company. It meets the performance requirements for “super demulsibility” as defined by Morgan’s Advanced Lubricant Specification, Revision 2.4, for use in hot and cold rolling mill operations. Bearing Oil M is formulated to provide rapid water separation, excellent oxidation resistance, protection against rust and corrosion, and resistance to foaming. It has excellent water-separating properties to minimize the formation of emulsions in circulating systems subject to contamination with large quantities of water, rolling solutions, dirt and scale. It has excellent oxidation resistance and thermal stability at high temperatures to minimize sludge and varnish formation, and provide long service life. It protects system components against rust and corrosion, and is resistant to excessive foam buildup that can interfere with proper lubrication.

Applications:

  • Backup roll bearings manufactured by Morgan Construction Company
  • Backup roll bearings in hot and cold rolling mills
  • Bearing lubrication in steel mills
  • Circulating systems where water contamination is a problem
  • Large, slow-speed gears in mixers and mills
Bearing Oil M meets the requirements of the following industry and OEM specifications:
  • Morgan Construction Advanced Lubricant Specification, Revision 2.4
  • SMS Siemag SN 180 Part 4 (07/2009)
  • U.S. Steel 135, Mill Circulating Oil
Features/Benefits:
  • Excellent water- separating properties
  • Excellent oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.878 g/cc
Density 7.32 lb/gal
Viscosity Measurement 98Index
Saybolt Viscosity at 100°F 788 SUS
Saybolt Viscosity at 210°F 78.9 SUS
Kinematic Viscosity at 40°C (104°F) 150 cSt
Kinematic Viscosity at 100°C (212°F) 14.8 cSt
Oxidative Stability 5.83 hourRPVOT; ASTM D2272
ASTM Color 2.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.050[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -20.0 °C
Flash Point 265 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility<1%Oil in Water, after centrifuging, UEC Dynamic Endurance Test
 <10%Water in Oil, after centrifuging, UEC Dynamic Endurance Test
 <20 minutes to passASTM D1401
 >30 mlFree Water @ 52°C, ASTM D2711

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5159 / 198412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.