MG266AI is a 20% mineral filled polypropylene compound intended for injection molding. This material has well balanced mechanical properties and high melt flow rate. Applications: MG266AI has been developed especially for the car industry to be used in automotive interior parts. - Automotive interior applications
- Door panels and pockets
- Interior trims
- Pillar trims
Special Features:- High flowability
- High stiffness
- Good surface aesthetics
- Easy processing
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.Information provided by Borealis AG |