System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Entec Hylex® P1317L1 HB Polycarbonate
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Optical Grade
Material Notes:
UV Stabilized, Higher Flow, Mold Release, Water Clear
Information provided by Entec.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.20
g/cc
ASTM D792
Water Absorption at Saturation
0.15 %
Immersion; ASTM D570
Linear Mold Shrinkage
0.005
-
0.007
cm/cm
ASTM D955
Melt Flow
17
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
70
ASTM D785
Tensile Strength at Break
10000
psi
ASTM D638
Elongation at Break
130 %
ASTM D638
Flexural Strength
13900
psi
ASTM D790
Flexural Modulus
340000
psi
ASTM D790
Izod Impact, Notched
13.0
ft-lb/in
ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.0e+17
ohm-cm
ASTM D257
Dielectric Strength
380
kV/in
ASTM D149
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
280
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
265
°F
ASTM D648
Flammability, UL94
HB
@Thickness 1.50 mm
HB
@Thickness 3.00 mm
Optical Properties
Original Value
Comments
Refractive Index
1.586
ASTM D542
Haze
1.0 %
ASTM D1003
Transmission, Visible
88 %
ASTM D1003
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release
Entec Hylex® P1310L1 HB Polycarbonate
Entec Hylex® P1325L1 HB Polycarbonate
Covestro Makrolon® 2607 Polycarbonate, Injection Grade
PENT063c / 142455
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.