Lewatit® MonoPlus SP 112 is a strongly acidic, macroporous cation exchange resin with beads of uniform size (monodisperse) based on a styrene-divinylbenzene copolymer. The monodisperse beads are chemically and osmotically very stable. The optimized kinetics leads to an increase operating capacity compared to ion exchange resins with heterodisperse bead size distribution. Lewatit MonoPlus SP112 is especially applicable for:- the demineralization of water for industrial steam generation e.g. Lewatit WS System, Lewatit Liftbed System or Lewatit Rinsebed System
- polishing by a Lewatit Multistep System in combination with Lewatit MonoPlus MP 800
- condensate softening
- condensate polishing in combination with Lewatit MonoPlus MP 800
- removal of cationic in process water stream (metal, plastics, etc.
Lewatit MonoPlus SP 112 is adding special features to the resin bed:high exchange flow rates during regeneration and loading- a good utilization of the total capacity
- a low demand for rinse water
- a homogeneous distribution of regenerants, water and solutions; leading to a homogeneous working zone
- a nearly linear pressure drop gradient for the whole bed depth; allowing higher bed depths