MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Henkel Loctite® Stycast® 2741 Two-Component Epoxy Flexible Encapsulant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: 2741 is designed for electronic embedment and in sealing or cementing of metals, ceramics and plastics. The hardness can be adjusted by varying the amount of Loctite CAT 15 used.Features:
  • Ease of use
  • Variable flexibility
  • General purpose
  • Room temperature cure capability
  • Shock and impact resistant
  • Room temp or heat cure

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³Part B, CAT 15
 1.15 g/cc0.0415 lb/in³Mixed
 1.65 g/cc0.0596 lb/in³Part A, Loctite Stycast 2741
Brookfield Viscosity 25000 cP25000 cPPart B, CAT 15
 36000 cP36000 cPMixed
 225000 cP225000 cPPart A, Loctite Stycast 2741
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inFlexible Material
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060Flexible Material
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FFlexible Material
Maximum Service Temperature, Air 65.0 °C149 °FFlexible Material
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Temperature 65.0 °C
2.00 - 4.00 hour
@Temperature 149 °F
Option 3
 240 - 360 min
@Temperature 45.0 °C
4.00 - 6.00 hour
@Temperature 113 °F
Option 2
 960 - 1440 min
@Temperature 25.0 °C
16.0 - 24.0 hour
@Temperature 77.0 °F
Option 1
Working Life 160 min
@Temperature 25.0 °C
160 min
@Temperature 77.0 °F
100 g
 
Descriptive Properties
AppearanceBlackPart B, CAT 15
 BlackPart A
Mix Ratio, by Volume250 : 100Loctite CAT 15 per 100 parts Loctite Stycast 2741
Mix Ratio, by Weight150 : 100Loctite CAT 15 per 100 parts Loctite Stycast 2741

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEMERS02 / 35694

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.