MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC LNP™ STAT-KON™ Compound DEL329E Polycarbonate (PC) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DEL329E compound is based on Polycarbonate (PC) resin containing 10% carbon fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Flame Retardant, Wear Resistant, Easy Molding.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Wear resistant,Electrically Conductive,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D792
Density 1.40 g/cc0.0506 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 93.0 MPa13500 psi5 mm/min; ISO 527
 95.0 MPa13800 psi5 mm/min; ASTM D638
Elongation at Break 2.2 %2.2 %5 mm/min; ASTM D638
 2.2 %2.2 %5 mm/min; ISO 527
Tensile Modulus 7.10 GPa1030 ksi1 mm/min; ISO 527
 7.36 GPa1070 ksi5 mm/min; ASTM D638
Flexural Strength 140 MPa20300 psiISO 178
 141 MPa20500 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 143 MPa20700 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.32 GPa917 ksi1.3 mm/min, 50 mm span; ASTM D790
 6.53 GPa947 ksi2 mm/min; ISO 178
Izod Impact Notched 66.0 J48.7 ft-lbASTM D256
Izod Impact, Unnotched 3.86 J/cm7.23 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 23.0 kJ/m²10.9 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 17.0 J12.5 ft-lbASTM D3763
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10 - 1.00e+6 ohm10 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
13.9 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 73.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
40.6 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 148 °C298 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 149 °C
@Thickness 3.20 mm
300 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 146 °C
@Thickness 3.20 mm
295 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81230 / 289177

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.