MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crucible Steel 316L Chromium-Nickel Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Crucible 316L is a non-hardenable, low carbon austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Crucible 316L is designed for special applications requiring resistance to sensitization and intergranular corrosion. This grade is non magnetic in annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.91 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 160
Tensile Strength, Ultimate 80000 psi
Tensile Strength, Yield 30000 psi
@Strain 0.2 %
Elongation at Break 55 %in 2"
Reduction of Area 65 %
Tensile Modulus 28000 ksi
Izod Impact Unnotched 100 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00007239 ohm-cm
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.90 µin/in-°F
@Temperature 0.000 - 100 °C
 9.00 µin/in-°F
@Temperature 0.000 - 316 °C
 10.3 µin/in-°F
@Temperature 0.000 - 649 °C
Specific Heat Capacity 0.120 BTU/lb-°F
@Temperature 0.000 - 100 °C
Thermal Conductivity 111.6 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 148.8 BTU-in/hr-ft²-°F
@Temperature 538 °C
Melting Point 2500 - 2550 °F
Solidus 2500 °F
Liquidus 2550 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 16 - 18 %
Iron, Fe >= 61.895 %As Remainder
Magnesium, Mg >= 3.0 %
Manganese, Mn <= 2.0 %
Molybdenum, Mo <= 2.0 %
Nickel, Ni 10 - 14 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 316L Austenitic Stainless steel
AISI Type 316L Stainless Steel, annealed sheet
AISI Type 316L Stainless Steel, annealed bar
AISI Type 316L Stainless Steel, annealed plate
AISI Type 316L Stainless Steel, annealed and cold drawn bar

NCRUC036 / 16029

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.