MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products BC 7062-3H Epoxy Casting
Categories: Polymer; Thermoset; Epoxy

Material Notes: BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yielding excessive shrinkage. Casting thicknesses may be increased by incorporating aluminum needles, puffs or granules. BC 7062, when properly cured, provides nearly perfect reproduction, resulting in a dimensionally stable, hard, tough surface. For use in constructing duplicate models, prototypes, patterns, facing dies, etc.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.72 g/cc
Brookfield Viscosity 3800 cP
@Temperature 23.9 °C
Mixed
Linear Mold Shrinkage 0.0027 cm/cmASTM D2566-69
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
@Temperature 23.9 °C
Tensile Strength, Ultimate 4500 psi
Flexural Strength 7200 psi
Compressive Strength 11000 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µin/in-°F
Heat Distortion Temperature 127 °F
 
Processing PropertiesOriginal ValueComments
Cure Time >= 2880 min
@Temperature 24.0 °C
Pot Life >= 240 min
@Temperature 24.0 °C
2 lb. mass
 
Descriptive Properties
MachinabilityExcellent
Mix Ratio6:1 by weight, 2.9:1 by volume, resin/harder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBCC039 / 107266

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.