Characteristics: Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications: Telecommunication equipment partsAutomotive electrical parts Moulding which remain in contact with metal partsElectric switchgear components ( eg. relay )Components exposed to warm atmosphere, etc.