MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bostik Dimension® RapidCure™ Grout
Categories: Other Engineering Material

Material Notes: Description: Dimension® RapidCure™ Glass-Filled, Pre-Mixed, Urethane Grout is a patented, reflective, water based, urethane grout. Dimension® RapidCure™ contains micro-glass beads and a translucent, urethane binder that both reflect light as well as allow it to pass through. This creates a variety of aesthetic effects in virtually all tile options available today. It may add an elegant sparkle and/or blend naturally with traditional tile and stone. It also creates a three dimensional effect within clear glass tile installations. Dimension® RapidCure™ is approved for intermittent water exposure after only 3 days of cure (see typical working properties chart for details).

Key Features:

  • Blends naturally with tile
  • No sealing required
  • 3 day water exposure

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.8 lb/gal
Volatile Organic Compounds (VOC) Content 35 g/lSCAQMD Rule #1168
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 510 psi
Compressive Strength 693 psiASTM C109
 >= 3500 psi
 3000 psi
@Time 259000 sec
Wet
 5000 psi
@Time 605000 sec
Dry
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourReady for Light Foot Traffic
 72.0 hourReady for Heavy Foot Traffic
 72.0 hourStain Resistance
 72.0 hourBefore Intermittent Water Exposure
Tack-Free Time 8.00 hour
Working Life 3.00 hour
Shelf Life 24.0 Month
 
Descriptive Properties
Chemical Resistance PropertiesAcetic Acid (3%)Pass per ASTM C267
 Ammonium ChloridePass per ASTM C267
 Citric Acid Solution (100 g/L)Pass per ASTM C267
 Hydrochloric Acid (10%)Pass per ASTM C267
 Lactic AcidPass per ASTM C267
 Phosphoric Acid (10%)Pass per ASTM C267
 Sodium Hypochlorite (1:1) 3%Pass per ASTM C267
 Sulfamic Acid (10%)Pass per ASTM C267
Installation Temperature4-38°C
Recycled Content60%pre-consumer recycled glass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bostik QuartzLock2™ RapidCure™ Urethane Grout
Bostik NeverSeal™ Grout
Bostik EzPoxy™ Epoxy Mortar & Grout
Concrete, Lightweight
CHT Group EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea

PBOSTK004 / 191540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.