MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
UBE UPILEX®-SGA 25SGA Polyimide
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: UPILEX®-SGA is a polyimide film having improved adhesion properties created by a special process to both sides of the UPILEX®-S. It is suitable for sputtering or plating processes because of high surface adhesion. It offers a flexible base for high-performance electronic circuits. In addition, it can also be used as an adhesive tape base material for LOC packaging. In sputtering or plating, a flexible base for electronic circuits that does not use any adhesives can be obtained. Peel strength is high, surface smoothness is very high. Superior mechanical property, with low water absorption, excellent dimensional stability and high heat resistance comparable to UPILEX®-S.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccASTM D1505
Water Absorption 1.2 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 490 MPaASTM D882
Elongation at Break 40 %ASTM D882
Tensile Modulus 10.0 GPaASTM D882
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmDC 100V; ASTM D257
Surface Resistance >= 1.00e+16 ohmDC 100V; ASTM D257
Dielectric Constant 3.4
@Frequency 1e+9 Hz
IPC-TM650 2.5.5.9
Dielectric Strength 6.40 kV/mmASTM D149
Dissipation Factor 0.0030
@Frequency 1e+9 Hz
IPC-TM650 2.5.5.9
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 50.0 - 200 °C
Fine linear dilatometer
Shrinkage 0.060 %
@Temperature 200 °C,
Time 7200 sec
heat; ASTM D1204

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PUBD9853 / 287316

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.