MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ELM® White Lithium Biodegradable Lubricating Grease
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Description: White Lithium Grease is premium quality biodegradable, Biotechbased™ multipurpose grease formulated from USA-grown vegetable oils and a lithiumbased thickener.

Applications:

  • Designed for protection between all metal to metal contact areas
  • Prevents rust and corrosion
  • Recommended for farm and plant machinery
  • Recommended for environmentally sensitive areas near waterways
Benefits:
  • White color helps differentiate new grease from old grease
  • Contains advanced extreme pressure additives for excellent protection
  • Reduces friction and wear
  • Superior lubricity lessens energy consumption and reduces heat
  • Higher flash point than petroleum greases for increased safety
  • Biodegradable formula reduces damage to the environment
  • Meets EPA’s Environmental Preferable Purchasing (EPP) criteria
  • Meets USDA’s proposed Biobased product definition for EO 13101
  • Manufactured from renewable USA-grown crop-based oils – Reduces foreign oil dependence

Information provided by ELM®

Key Words: NLGI GRADE 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity at 40°C (104°F) 51 cSt51 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)
Four Ball Wear 0.540 mm0.0213 in
Penetration 265 - 295265 - 295Cone, worked 60 strokes
Oil Separation <= 5.0 %<= 5.0 %
 
Thermal PropertiesMetricEnglishComments
Flash Point 326 °C619 °FBase Oil
Dropping Point 170 °C338 °F
 
Descriptive Properties
AppearanceWhite to Off-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubriplate Lithium Brick Grease Specialty Lubricant and Grease
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 2
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 3
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 2
ELM® SoyGrease™ Biodegradable Grease for Semi-Truck Fifth Wheels

WELML004 / 146207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.