MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Xyron™ AG211 PA/PPE
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: Excellent heat resistance, flame retardance, dimensional stability, and mechanical properties. Applications: Automotive parts, electrical & electronic parts, industrial parts.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccISO 1183
Filler Content 10 %10 %
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in120X80X3mm; Asahi Kasei
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 94.0 MPa13600 psi50% RH; ISO 527
Elongation at Break 5.0 %5.0 %50%RH; ISO 527
Flexural Strength 148 MPa21500 psi50% RH; ISO 178
Flexural Modulus 3.70 GPa537 ksi50% RH; ISO 178
Charpy Impact, Notched 1.10 J/cm²
@Thickness 4.00 mm
5.23 ft-lb/in²
@Thickness 0.157 in
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature -30.0 - 65.0 °C
27.8 µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 199 °C390 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FResin Temperature
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature 110 - 130 °C
@Time 7200 - 14400 sec
230 - 266 °F
@Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Xyron™ G702H PPE/PS, Glass Fiber Reinforced

PASAHI8242 / 221269

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.