MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 5430 Squeak Reduction Tape
Categories: Polymer; Tape

Material Notes: 3M™ Squeak Reduction Tapes are a film tape for the automotive industry to help control squeaks and rattles due to vibration or wear of metal and plastic materials.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.010 %
Thickness 3.20 milLiner; ASTM D3752
 5.00 milBacking; ASTM D3752
 7.00 milTotal without liner; ASTM D3752
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38.7 MPaASTM D3759
Elongation at Break 175 %ASTM D3759
Peel Strength 4.6875 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 107 °C
Minimum Service Temperature, Air -34.0 °C
 
Descriptive Properties
Adhesive TypeAcrylic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 5430 Low Density Polyethylene, Cast Film
Ineos Nova 5420 High Impact Polystyrene
SIDPEC EGYPTENE® HD 5420 GA HDPE Blow Molding
Henkel Loctite® 5420 Heat Cure Form-In-Place Electrically Conductive Silicone Sealant
Celanese SO.F.TER Sofprene T® 5420.A96 SBS TPE

PMM34545 / 169292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.